Got some issues here that I seemingly cannot solve, any Inputs?
>Filament is sometimes overextruded and underextruded other times, on the same prints
>Ragged Edges on one side, clean edges on the other side of the same prints
>Print walls have uneven thickness and sometimes seperate after a few days
Filament is Amazon Basics PETG, I print with 250°C because some Anons told me printing too cold would cause weak layer strength. I could crank it up to 300°C (full metal hotend), but I don't know I wat to heat up PETG any higher than 250°C.

I've already tuned E-Steps to a ridiculous degree, the hotend is new (https://www.amazon.de/dp/B0B2ZMJMDW)) because the old one just leaked petg out of every hole.

I also have problems with bed adhesion sometimes, but that's another issue.