Hi!
I'm back again from one year hibernation.
I'm trying to print this piece, but every time it lifts at the corners and inside the hole. I'm using 60°C glass plate and hairspray with 190°PLA.
I even tried with the blue tape but same result. It lifts right away tearing the tape.
You can clearly see in pic related where it stayed adhered on the plate and where it lifted (especially around that square hole).
What can I do to contrast this?
It's a big piece to print (16 h) and I'm scared of the idea of the piece just lifing on the final layers