if you strip galv off with hydrochloric acid it makes killed spirits, a potent soldering flux. excellent for soldering ends on bowden cables.

>> No.1281495 [View]
File: 897 KB, 2304x1728, DSCF1291.jpg [View same] [iqdb] [saucenao] [google]
1281495

>>1281048
when i'm making bowden cables from stainless, i use ordinary 60/40 in a solder pot with 85% phosphoric acid as a dip flux.
the acid cloud is fucking brutal, make sure you use your safety lean and safety squint.